Blended apparel
Polyester-blend fabric
Generic / JPPlus guidance
Temperature375–390°F191–199°C
Time55 sec–1 min 5 sec
Pressurelight medium
Verify before production. This result assumes the cited product scope. Test with the actual press, transfer system, blank lot, environment, and production conditions.
Preparation
- Confirm polyester content and expected muted result.
- Lint-roll and pre-press for moisture.
Removal and cooling
- Paper removal
- Lift without sliding.
- Cooling
- Cool flat before stacking.
Scope and caveats
- Lower polyester content produces lower dye yield.
- Blend chemistry can increase scorching or dye-migration risk.
Evidence
Sources
- Johnson Plastics Plus — Sublimation Settings: Time, Temperature, & PressureOfficial source · last checked 2026-08-04